The clear tubes that I use are Pyrex.

The problem with the pens is that unlike the glass, it only has one size. And for the pens and the Pyrex, most of the dogbones were not entirely round. The ones needed here have a flat side so molding them is the only way to get an authentic look. I have actually tried plastic. It tends to melt when the component is soldered in place. You must be careful with heat. Also, use flat paint on the plastic or glass or it comes out way-shiny. You can also rough-up the plastic and the glass for adhesion and a better look.